MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® POM-C EC POM-C + conductive carbon black
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: This POM-C contains conductive carbon black and is thus electrically conductive. It is therefore particularly suited to applications in the safety sector, explosion protection field (e.g. ATEX), electronic protection, transport and mechanical conveying and handling, etc.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccDIN EN ISO 1183-1
Moisture Absorption 0.250 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 79DIN EN ISO 868
Ball Indentation Hardness 100 MPaDIN EN ISO 2039-1
Tensile Strength, Yield 40.0 MPa50 mm/min; DIN EN ISO 527
Elongation at Break 30 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 1.90 GPa1 mm/min; DIN EN ISO 527
Charpy Impact, Notched 5.00 kJ/m²DIN EN ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5000 ohm-cmIEC 60093
Surface Resistance 1000 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 130 µm/m-°C
@Temperature 23.0 - 60.0 °C
DIN 53752
Thermal Conductivity 0.310 W/m-K
Melting Point 165 °CISO 11357-3
Maximum Service Temperature, Air 100 °Cshort term
 140 °Clong term
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °CDIN EN ISO 75/A
Minimum Service Temperature, Air -20.0 °C
Flammability, UL94 HB
@Thickness 3.00 mm
 HB
@Thickness 6.00 mm
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP041 / 250539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.