MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ovako 21CrMoV5-7 6130 Steel, +QT
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: 21CrMoV5-7 is a steel for fasteners with specified elevated and/or low temperature properties. Imanite has been designed for nitriding, giving similar hardness distribution as case hardening. When using nitriding the distortion due to quenching after carburising can be avoided. Imanite is a M-steel version of 21CrMoV5-7 . M-treatment is very beneficial when the machining is done in Q&T condition and the hardness is about 300 HBW.

Information provided by Ovako

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 205 - 250
@Thickness 25.0 - 160 mm
205 - 250
@Thickness 0.984 - 6.30 in
Tensile Strength 700 - 850 MPa
@Thickness 25.0 - 160 mm
102000 - 123000 psi
@Thickness 0.984 - 6.30 in
Tensile Strength, Yield >= 550 MPa
@Thickness 25.0 - 160 mm
>= 79800 psi
@Thickness 0.984 - 6.30 in
Elongation at Break 16 %
@Thickness 25.0 - 160 mm
16 %
@Thickness 0.984 - 6.30 in
Reduction of Area 60 %
@Thickness 25.0 - 160 mm
60 %
@Thickness 0.984 - 6.30 in
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.300.30
Shear Modulus 80.0 GPa11600 ksi
Impact Test 63.0 J
@Thickness 25.0 - 160 mm,
Temperature 20.0 °C
46.5 ft-lb
@Thickness 0.984 - 6.30 in,
Temperature 68.0 °F
long
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
6.67 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
0.110 - 0.115 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
Transformation Temperature 405 °C761 °FMS
 745 °C1370 °FAC1
 853 °C1570 °FAC3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.17 - 0.25 %0.17 - 0.25 %
Chromium, Cr 1.2 - 1.5 %1.2 - 1.5 %
Iron, Fe 95.84 - 97.28 %95.84 - 97.28 %As Balance
Manganese, Mn 0.40 - 0.80 %0.40 - 0.80 %
Molybdenum, Mo 0.55 - 0.80 %0.55 - 0.80 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.15 - 0.40 %0.15 - 0.40 %
Sulfur, S <= 0.030 %<= 0.030 %
Vanadium, V 0.25 - 0.35 %0.25 - 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 705°C (1300°F) temper, 25 mm (1 in.) round
AISI 5120H Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 775°C (1430°F), 150°C (300°F) temper
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 650°C (1200°F) temper, 25 mm (1 in.) round
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 540°C (1000°F) temper, 25 mm (1 in.) round

NOVAKO168 / 234467

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.