MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Polyrocks Chemical 168B Polypropylene, halogen-free flame retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: 168B is flame retardant polypropylene with bromine and antimony as the flame retardant elements. Through gas-phase mechanism play the flame retardant performance. 168B flammability can reach UL 94 V-2(1.5mm and 3.0mm),glow-wire test meets GWIT:775/3.0 and GWFI:850/3.0? 168B has characteristics of good flowability?strong chemical resistance?good mechanical properties...etc.

Information provided by Polyrocks

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D792
Linear Mold Shrinkage 0.014 - 0.018 cm/cm0.014 - 0.018 in/inASTM D955-08
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 35.0 MPa5080 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Flexural Strength 40.0 MPa5800 psiASTM D790
Flexural Modulus 1.40 GPa203 ksiASTM D790
Izod Impact, Notched 0.350 J/cm0.656 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
Glow Wire Ignition Temperature 775 °C
@Thickness 3.00 mm
1430 °F
@Thickness 0.118 in
Pass; IEC 60695-2-13
Glow Wire Flammability Index 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
Pass; IEC 60695-2-13
 
Descriptive Properties
Ball Pressure1.75-1.90 mmIEC 60695-10-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPROCKS010 / 278518

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.