MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lubrizol Advanced Materials Pearlstick® 48-60/03 Linear Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pearlstick® 48-60/03 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low-medium thermoplasticity level, available as pellets.

Solubility: Pearlstick® 48-60/03 is soluble in acetone, methyl ethyl ketone (MEK), cyclohexanone, dimethyl formamide and tetrahydrofuran (THF). Diluting solvents such as toluene and ethyl acetate can be added.

The solvents and diluents should be water-free (max 0.1%), so as to avoid subsequent side reactions during crosslinking with isocyanates.

Solutions: Pearlstick® 48-60/03 gives transparent solutions. It should be dissolved in closed tanks, and the use of high shear equipment is advised. The final viscosity figures can vary, depending on the stirring process and on the solvent/diluents ratios.

Applications: Pearlstick® 48-60/03 is used for the production of adhesives for bonding plasticized PVC to plasticized PVC or other materials such as leather, textiles, rubber, etc.

Pearlstick® 48-60/03 enables the production of adhesives with high solids content and low viscosity, which are intended for spray application in the automotive industry and with high performances in the green-strength of the joints and temperature resistance. The addition of a poly-functional isocyanate improves the heat-resistance and the strength of the joints.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccISO 2781
Brookfield Viscosity 200 - 400 cP
@Temperature 20.0 °C
200 - 400 cP
@Temperature 68.0 °F
Brookfield RVF sp. 3, 20 rpm solution at 15% in MEK; MQSA N0 40A
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 60.0 °C>= 140 °FActivation Temperature; EN-12961
 
Descriptive Properties
Colorwhite or slightly yellowish
Crystallization RateVery High
Freezing ResistanceVery goodMQSA 90
Heat ResistanceExcellentMQSA 11E
Hydroxyl ContentApprox. 0.1%MQSA 47A
Solubility - Acetone / Ethyl Acetate0:100
Solubility - Acetone / Toluene10:90
Solubility - MEK / Toluene20:80
Solubility - MEK/ Ethyl Acetate0:100
Thermoplasticity RangeLow-medium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMEQU982 / 109219

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.