MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis BorSafe™ HE3490-LS-HW HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: BorSafe" HE3490-LS-HW is a bimodal polyethylene compound produced by the advanced Borstar technology. The product is a high-density polyethylene compound in pellet form and contains a combination of stabilizers and carbon black to ensure a reliable long-term stability and UV-resistance. BorSafe HE3490-LS-HW is classified as an MRS 10.0 material (PE100) and is PE100-RC classified following the draft EN/ISO PE pressure pipe standards as currently revised.

Applications:

  • Drinking water
  • Sheets and profiles
  • Gas distribution
  • Cable protection pipes
  • Industrial applications
  • Co-extrusion of layers for pressure pipes
  • Relining
  • Corrugated pipes
Specifications:
  • EN 12201
  • ISO 4427
  • EN 1555
  • ISO 4437
  • EN ISO 15494

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.9575 g/cc0.03459 lb/in³ISO 1183-1/Method A
Oxidative Induction Time (OIT) >= 20.0 min
@Temperature 210 °C
>= 20.0 min
@Temperature 410 °F
ISO 11357-6
Carbon Black Loading 2.00 - 2.50 %2.00 - 2.50 %ISO 6964
 <= 3.00 %<= 3.00 %dispersion; ISO 18553
Melt Flow 0.220 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.220 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 50.0 °C<= 122 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.0 MPa3480 psi50 mm/min; ISO 527-2
Elongation at Break >= 600 %>= 600 %50 mm/min; ISO 527-2
Tensile Modulus 1.05 GPa152 ksi1 mm/min; ISO 527-2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 210 °C374 - 410 °FCylinder
Die Temperature 200 - 210 °C392 - 410 °F
Melt Temperature 190 - 220 °C374 - 428 °F
Head Temperature 200 - 210 °C392 - 410 °F
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Accelerated Full Notch Creep Test>550 hin 2% Dehyton solution (4 MPa, 90 °C); ISO 16770
Accelerated Notched Pipe Test>300 hin 2% Arkopal N-100 solution (9,2 bar, 80 °C); ISO 13479
Cracked Round Bar>1.5 Million cyclesconverted to 14,0 mm and initial crack length 1,40 mm (12,5 MPa, 23°C); ISO 18489
Resistance to rapid crack propagation>10 barS4 test, Pc at 0°C, Test pipe 250mm, SDR11; ISO 13477
Strain Hardening Modulus Test65 MPaISO 18488

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9658 / 323015

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.