Description: Pro-fax™ SG722 high flow, high impact polypropylene copolymer resin is designed for injection molding applications. This resin is available in pellet form. Pro-fax™ SG722 resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520, for food contact, including cooking applications. All ingredients in Pro-fax™ SG722 resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Household goods, toys, consumer applications, sporting goods Information provided by Basell. |