MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.5 PHR Thanecure ZM
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.

Thanecure ZM is an activator for a sulfur cure of Millathane® millable polyurethanes consisting of a partial complex of zinc chloride and MBTS.

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6969
Tensile Strength 33.2 MPa4820 psi
Elongation at Break 600 %600 %
100% Modulus 3.22 MPa
@Strain 100 %
467 psi
@Strain 100 %
200% Modulus 7.343 MPa
@Strain 200 %
1065 psi
@Strain 200 %
300% Modulus 12.98 MPa
@Strain 300 %
1882 psi
@Strain 300 %
Tear Strength 62.5 kN/m357 pliDie C
Compression Set 32.1 %
@Temperature 70.0 °C,
Time 79200 sec
32.1 %
@Temperature 158 °F,
Time 22.0 hour
 
Processing PropertiesMetricEnglishComments
Cure Time 12.4 min
@Temperature 155 °C
0.207 hour
@Temperature 311 °F
TC90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TSE Industries Millathane® 66 Millable Polyurethane Rubber
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer
Sawbones Solid Rigid Polyurethane Foam 50 pcf Density
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density
Sawbones Solid Rigid Polyurethane Foam 30 pcf Density

PMILL019 / 87063

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.