MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion Yttrium Fluoride, YF3
Categories: Ceramic; Halide

Material Notes: Yttrium Fluoride, YF3, produces low-index film layers that exhibit good transparency in the UV through infrared regions. The films are insoluble and show low stress, making YF3 a useful substitute for ThF in many IR applications. It can be combined in multilayers with other fluoride compounds and with higher-index ZnS and ZnSe layers for AR and filter coatings out to wavelengths >10 µm. Its absorption at 10.6 µm is low, but limits its use to laser applications that do not require the highest damage thresholds.

Film Properties: Yttrium Fluoride films can be deposited from the melt by resistance-heated or electron beam evaporation. Film density and refractive index increase with substrate temperature. Thicknesses greater than 2 µm will adhere to Zinc Sulfide, glass, and Germanium substrates heated to 250°C. Yttrium Fluoride is insoluble, therefore making it suitable for humid conditions when applied hot. Water absorption bands of depth 2-5% are present at 2.8-3.2 µm and 5.6 -7.3 µm on colder substrates. When used in multi-layer combination with ZnS or ZnSe, the substrate temperature must be reduced to ~175°C to avoid the low sticking coefficients that those materials exhibit at higher temperatures. Amorphous films exhibiting low scatter can be deposited below 150°C substrate temperature, but adhesion and refractive index properties are compromised. Above ~250°C, the films become crystalline and harder, but they exhibit noticeable scatter and are more highly stressed.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.01 g/cc0.145 lb/in³Crystal
Molecular Weight 145.9 g/mol145.9 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 1387 °C2529 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.29
@Wavelength 10500 nm
1.29
@Wavelength 10500 nm
 1.325
@Wavelength 9500 nm
1.325
@Wavelength 9500 nm
 1.35
@Wavelength 8500 nm
1.35
@Wavelength 8500 nm
 1.395
@Wavelength 7500 nm
1.395
@Wavelength 7500 nm
 1.465
@Wavelength 6500 nm
1.465
@Wavelength 6500 nm
 1.475
@Wavelength 4500 nm
1.475
@Wavelength 4500 nm
 1.475
@Wavelength 5500 nm
1.475
@Wavelength 5500 nm
 1.488
@Wavelength 3500 nm
1.488
@Wavelength 3500 nm
 1.49
@Wavelength 2500 nm
1.49
@Wavelength 2500 nm
 1.495
@Wavelength 1500 nm
1.495
@Wavelength 1500 nm
 1.51
@Wavelength 500 nm
1.51
@Wavelength 500 nm
 
Descriptive Properties
ColorWhite
Evaporation Temperature900°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMATER915 / 323621

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.