MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay Engineered Polymers SEQUEL® 5220 Engineered Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Description: SEQUEL® 5220 engineered polyolefin is designed for large exterior applications that require superior painted gouge/scuff performance. This product also offers ductile impact properties at low temperatures, excellent paintability, and processability.

Applications: Bumper fascias, claddings

Information provided by Solvay Engineered Polymers.

LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/ccISO 1183
Linear Mold Shrinkage 0.013 - 0.015 cm/cm0.013 - 0.015 in/inafter bake; ISO 294
Melt Flow 20.2 g/10 min20.2 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.5 MPa3120 psi150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.70 GPa247 ksi80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 24.0 J17.7 ft-lbmultiaxial, 2.2 m/s; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 68.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
37.8 µin/in-°F
@Temperature -22.0 - 176 °F
ASTM E228

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOLE25 / 68031

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.