MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rotuba 860H2 Ethyl Cellulose
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Ethyl Cellulose, Molded

Material Notes:

Data provided by the manufacturer.

Key Words: Rotuba Plastics; Cellulosic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccASTM D792-60T
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 112ASTM D785
Tensile Strength, Ultimate 48.0 MPaASTM D638-61T
Elongation at Break 22 %ASTM D638-61T
Izod Impact, Notched 0.960 J/cmASTM D256-56
 0.270 J/cm
@Temperature -40.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.18
@Frequency 10000 Hz
ASTM D150-54T
 3.23
@Frequency 1000 Hz
ASTM D150-54T
Dissipation Factor 0.0072
@Frequency 1000 Hz
ASTM D150-54T
 0.0127
@Frequency 10000 Hz
ASTM D150-54T
 
Thermal PropertiesOriginal ValueComments
Melting Point 155 °CFlow temperature, ASTM D569-59
Deflection Temperature at 0.46 MPa (66 psi) 102 °CASTM D648-56

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Ethyl Cellulose, Molded
Rotuba 860H Ethyl Cellulose
Rotuba 860S Ethyl Cellulose
Rotuba 860MH 686.4 Ethyl Cellulose
Rotuba 860M Ethyl Cellulose

PECR16 / 35492

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.