MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
International Mold Steel Premium H13 Hot Work Die and Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Hot Work Steel; Mold Steel

Material Notes: Description: International Mold Steel's Premium H-13 is a chromium-based, hot work die and plastic mold steel designed for increased production rates and longer tool life. It meets the restrictive standards of the North American Die Casting Association and other industrial specifications such as Chrysler's NP2080 for die casting applications. International Mold Steel's Premium H-13 is used for extended production runs that focus on reliability and consistency in the die or mold steel to minimize costly downtime. The manufacture of this die and mold steel begins with exacting chemistry control including very low sulfur level to increase toughness properties and resistance to heat checking. It is remelted to optimize steel integrity followed by special thermal processing for the development of homogeneous microstructure with uniformly distributed carbides. This provides the die caster or molder with outstanding ductility throughout large sections, which is essential to resist cleavage cracking under more demanding operating conditions.

Unique Characteristics:

  • Thermal shock and fatigue resistant
  • Meets NADCA, Chrysler and Mold Quality specifications
  • Superior machinability and polishability.

Applications: Aluminum extrusion , Die-casting inserts, Bending , Ejector pins, Die casting , Extrusion rams, Forging , Extrusion press liners, Gripper , Hot piercers, Hot heading , Hot shears, Hot press , Hot work mandrels, Hot trimmer , Hot work punches, Plastic mold , Plungers, Rivet Swaging , Sleeves slides

Information provided by International Mold Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.761 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 46
Tensile Strength, Ultimate 218000 psi
Tensile Strength, Yield 204000 psi
Elongation at Break 13 %Elongation in 2"
Reduction of Area 47 %
Modulus of Elasticity 30000 ksiat RT
Machinability 70 %of a 1% Carbon tool steel (annealed), which has a rating of 60% of B1112 Bessemer screw stock
Izod Impact 27.0 J
@Temperature 22.0 °C
 37.0 J
@Temperature 149 °C
 46.0 J
@Temperature 371 °C
Charpy Impact 19.0 ft-lbV-Notch
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.80 µin/in-°F
@Temperature 26.7 - 93.3 °C
 6.30 µin/in-°F
@Temperature 26.7 - 204 °C
 6.90 µin/in-°F
@Temperature 26.7 - 427 °C
Thermal Conductivity 17.6 W/m-K
@Temperature 27.0 °C
 23.4 W/m-K
@Temperature 204 °C
 26.8 W/m-K
@Temperature 649 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.40 %
Chromium, Cr 5.25 %
Iron, Fe 90.6 %
Manganese, Mn 0.40 %
Molybdenum, Mo 1.35 %
Silicon, Si 1.0 %
Vanadium, V 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type H13 Hot Work Tool Steel
AISI Type P20 Mold Steel (UNS T51620)
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel
International Mold Steel NAK55 Precipitation Hardened Mold Steel
Assab Steels MOLDMAX LH/MM Copper Alloy for Plastic Molds

NIMS06 / 17385

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.