MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Constellium Alumold® 110 Aluminum Cast Sliced Plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The material properties are enhanced by its stringent casting process which considerably reduces porosity throughout the thickness of the plate.

Information provided by manufacturer

Key Words: EN AW-5083; AlMg4.5Mn0.7
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.66 g/cc0.0961 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  70
@Thickness 150 - 500 mm
70
@Thickness 5.91 - 19.7 in
 70
@Thickness 500 - 600 mm
70
@Thickness 19.7 - 23.6 in
Tensile Strength  >= 210 MPa
@Thickness 150 - 500 mm
>= 30500 psi
@Thickness 5.91 - 19.7 in
Temper 03
 >= 210 MPa
@Thickness 500 - 600 mm
>= 30500 psi
@Thickness 19.7 - 23.6 in
Temper 03
 235 MPa
@Thickness 150 - 500 mm
34100 psi
@Thickness 5.91 - 19.7 in
Typical Strength
 235 MPa
@Thickness 500 - 600 mm
34100 psi
@Thickness 19.7 - 23.6 in
Typical Strength
Tensile Strength, Yield  >= 110 MPa
@Strain 0.2 %,
Thickness 150 - 500 mm
>= 16000 psi
@Strain 0.2 %,
Thickness 5.91 - 19.7 in
Temper 03
 >= 110 MPa
@Strain 0.2 %,
Thickness 500 - 600 mm
>= 16000 psi
@Strain 0.2 %,
Thickness 19.7 - 23.6 in
Temper 03
 115 MPa
@Strain 0.2 %,
Thickness 150 - 500 mm
16700 psi
@Strain 0.2 %,
Thickness 5.91 - 19.7 in
Typical Strength
 115 MPa
@Strain 0.2 %,
Thickness 500 - 600 mm
16700 psi
@Strain 0.2 %,
Thickness 19.7 - 23.6 in
Typical Strength
Elongation at Break  >= 5.0 %
@Thickness 150 - 500 mm
>= 5.0 %
@Thickness 5.91 - 19.7 in
Temper 03
 >= 5.0 %
@Thickness 500 - 600 mm
>= 5.0 %
@Thickness 19.7 - 23.6 in
Temper 03
 9.5 %
@Thickness 150 - 500 mm
9.5 %
@Thickness 5.91 - 19.7 in
Typical Elongation
 9.5 %
@Thickness 500 - 600 mm
9.5 %
@Thickness 19.7 - 23.6 in
Typical Elongation
Modulus of Elasticity 71.0 GPa10300 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000580 - 0.00000660 ohm-cm0.00000580 - 0.00000660 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.8 µm/m-°C
@Temperature 20.0 - 100 °C
13.2 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 105 - 120 W/m-K729 - 833 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 92.55 - 95.55 %92.55 - 95.55 %as balance
Chromium, Cr 0.050 - 0.25 %0.050 - 0.25 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg 4.0 - 4.9 %4.0 - 4.9 %
Manganese, Mn 0.40 - 1.0 %0.40 - 1.0 %
Silicon, Si <= 0.40 %<= 0.40 %
Zinc, Zn <= 0.25 %<= 0.25 %
Zr+Ti <= 0.15 %<= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ALIMEX ACP 5080 Aluminum Cast Plate
ALIMEX ACP 5080R Aluminum Cast Material
Constellium Fibral® Cast Aluminum Sliced Plate
Constellium PLAN 5083 Aluminum Rolled Plate
Alclad Aluminum 6061-O

NCONS011 / 160274

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.