Pro-fax SB786 impact polypropylene copolymer is available in pellet form. This resin is typically used in injection molding applications and offers good cold temperature impact and blush resistance. ASTM and ISO-based versions of the technical data sheet are available for Pro-fax SB786. Availability: North America Application: Battery Cases Market: Automotive; Industrial Packaging Processing Method: Injection Molding Attribute: Blush Resistant; Good Stiffness; Low Temperature Impact Resistance Information provided by LyondellBasell. |