  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Chemlon® 113 GHIU BK156 Nylon 66, 13% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Availability: Europe; Asia Pacific; North America

Fillers/Reinforcement: Glass Fiber 13% Filler by Weight

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Maximum Moisture Content 0.200.20
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inISO 527-2
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 100 MPa14500 psiISO 527-2
Elongation at Break 2.5 %2.5 %ISO 527-2
Elongation at Yield 2.5 %2.5 %ISO 527-2
Flexural Strength 150 MPa21800 psiISO 178
Flexural Modulus 4.83 GPa701 ksiISO 178
Izod Impact, Notched (ISO) 7.98 kJ/m²3.80 ft-lb/in²ISO 180/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmISO 1325
Dielectric Strength 18.1 kV/mm
@Thickness 3.00 mm
460 kV/in
@Thickness 0.118 in
ASTM D149
Comparative Tracking Index 600 V600 VUL 746
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 214 °C417 °FUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 0.762 mm
HB
@Thickness 0.0300 in
Oxygen Index 25 %25 %ISO 4589-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 241 - 257 °C465 - 495 °F
Middle Barrel Temperature 257 - 271 °C495 - 520 °F
Front Barrel Temperature 263 - 279 °C505 - 535 °F
Nozzle Temperature 263 - 282 °C505 - 540 °F
Melt Temperature 257 °C495 °F
 263 - 282 °C505 - 540 °F
Drying Temperature 79.4 °C175 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber
Celanese Crastin® SK609 BK851 PBT-GF50

PTEKNQ0449 / 236940

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.