MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Aquathene CM04483 W&C Polyolefin Compound
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Aquathene CM04483 is a catalyst masterbatch selected by customers for fast curing moisture cure applications. In addition to catalyst, CM04483 also contains antioxidants and metal deactivator. When melt blended at 5 wt% to Aquathene AQ120000, the resulting material is capable of crosslinking when exposed to moisture.

Availability: North America

Application: Wire & Cable

Market: Wire & Cable

Processing Method: Wire & Cable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.932 g/cc0.0337 lb/in³ASTM D1505
Melt Flow 13.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
13.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9043 / 323971

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.