MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Evonik MHOROMER® Ultra High Purity HEMA 2-Hydroxyethyl Methacrylate  (discontinued **)
Categories: Fluid

Material Notes: Application: Basic monomer for soft contact lenses.

Appearance: Clear, colorless liquid.

Odor: Ester-like

CAS: 868-77-9

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³
Viscosity 5.0 cP
@Temperature 30.0 °C
5.0 cP
@Temperature 86.0 °F
Molecular Weight 130.1 g/mol130.1 g/mol
Vapor Pressure 0.000100 bar
@Temperature 20.0 °C
0.0750 torr
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.050<= 0.050Rohm Method: STM 05 (acid-base titration, as MAAC)
 
Thermal PropertiesMetricEnglishComments
Boiling Point 250 °C
@Pressure 0.1013 MPa
482 °F
@Pressure 14.69 psi
Flash Point 101 °C214 °FDIN 51758
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.453
@Temperature 20.0 °C
1.453
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.10 %<= 0.10 %Rohm Method: STM 07 (K. Fischer)
 
Descriptive Properties
Colormax. 5Rohm Method: STM 08 (Pt-Co)
Degree of Purity (%)min. 99.6Rohm Method: STM 13
Ethylene glycol dimethacrylate (%)max. 0.1Rohm Method: STM 03 (GC)
Heat of Polymerization (kJ/mol)50
MEHQ25-35ppm, Rohm Method: STM 04 (Photometric)
Polyethylene glycol monomethacrylates (%)max. 0.15Rohm Method: STM 03 (GC)
Solidification Point (°C)below -60

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age
Evonik MHOROMER® AM 101 Ethyl Methacrylate
ATI Allvac® 6-4ELI Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
ATI Allvac® 6-4 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
E-CRGlas® Fiber

PCYR00080 / 101069

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.