MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chemours Teflon™ Type LP, general purpose PFA film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Teflon™ PFA film is a transparent, thermoplastic film that can be heat sealed, thermoformed, vacuum formed, heat bonded, welded, metallized, laminated (combined with dozens of other materials), and used as an excellent hot-melt adhesive. This wide variety of fabrication possibilities combines with the following important properties to offer a unique balance of capabilities not available in any other plastic film. Teflon™ PFA film is chemically inert and solvent-resistant to virtually all chemicals, except molten alkali metals, gaseous fluorine, and certain complex halogenated compounds, such as chlorine trifluoride at elevated temperatures and pressures. It also has low permeability to liquids, gases, moisture, and organic vapors. Features: Chemical Compatibility, Electrical Reliability, Wide Thermal Range, Mechanical Toughness, Long Time Weatherability, Reliability. The convenience of Teflon™ PFA fluoropolymer in easy-to-use film facilitates the design and fabrication of this low friction thermoplastic for all sorts of high performance jobs. It is transparent and can be heat sealed, thermoformed, welded, and heat bonded. Superior anti-stick properties make it an ideal release film for many applications. A cementable type with an invisible surface treatment is available for bonding to one or both sides with adhesives.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.15 g/cc0.0777 lb/in³ASTM D1505
Water Absorption <= 0.030 %
@Time 86400 sec
<= 0.030 %
@Time 24.0 hour
ASTM D570
Moisture Absorption <= 0.0200 %<= 0.0200 %
Specific Surface Area 0.15 m²/g0.15 m²/g
 0.20 m²/g0.20 m²/g
 0.30 m²/g0.30 m²/g
 0.95 m²/g0.95 m²/g
 1.9 m²/g1.9 m²/g
 3.8 m²/g3.8 m²/g
 6.4 m²/g6.4 m²/g
 9.0 m²/g9.0 m²/g
 18 m²/g18 m²/g
 36 m²/g36 m²/g
Water Vapor Transmission 2.02 g/m²/day0.130 g/100 in²/dayASTM E96
Oxygen Transmission 6700 cc-mm/m²-24hr-atm17000 cc-mil/100 in²-24hr-atmASTM D1434
Nitrogen Transmission 2000 cc-mm/m²-24hr-atm5080 cc-mil/100 in²-24hr-atmASTM D1434
Carbon Dioxide Transmission 14000 cc-mm/m²-24hr-atm35600 cc-mil/100 in²-24hr-atmASTM D1434
Thickness 12.7 microns0.500 mil
 25.4 microns1.00 mil
 50.8 microns2.00 mil
 76.2 microns3.00 mil
 127 microns5.00 mil
 254 microns10.0 mil
 508 microns20.0 mil
 1520 microns60.0 mil
 2290 microns90.0 mil
 3180 microns125 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength at Break 20.7 MPa3000 psiASTM D882
Tensile Strength 25.0 MPa3630 psiASTM D1457
Tensile Strength, Yield 12.0 MPa1740 psiASTM D882
Elongation at Break 300 %300 %ASTM D882
Modulus of Elasticity 0.483 GPa70.0 ksiASTM D882
Flexural Modulus 0.586 GPa85.0 ksiASTM D790
Flex Crack Resistance 100000100000Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched NBNBASTM D256
Tensile Impact 620 J/cm1160 ft-lb/inChemours pneumatic impact tester
Coefficient of Friction, Dynamic 0.10 - 0.300.10 - 0.30Film-to-Steel; ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+17 ohm-cm
@Temperature -40.0 - 240 °C
>= 1.00e+17 ohm-cm
@Temperature -40.0 - 464 °F
ASTM D257
Surface Resistivity per Square >= 1.00e+17 ohm>= 1.00e+17 ohmASTM D257
Dielectric Constant 2.0
@Frequency 100 - 1.00e+6 Hz,
Temperature 25.0 °C
2.0
@Frequency 100 - 1.00e+6 Hz,
Temperature 77.0 °F
ASTM D150
Dielectric Strength 260 kV/mm
@Thickness 0.0250 mm
6600 kV/in
@Thickness 0.000984 in
Short-time, in air; ASTM D149 Method A
Dissipation Factor 0.00020 - 0.00070
@Frequency 100 - 1.00e+6 Hz
0.00020 - 0.00070
@Frequency 100 - 1.00e+6 Hz
ASTM D150
Arc Resistance >= 180 sec>= 180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°F
Thermal Conductivity 0.195 W/m-K1.35 BTU-in/hr-ft²-°FCenco-Fitch
Melting Point 302 - 310 °C576 - 590 °FASTM D3418
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.351.35ASTM D542
Transmission, Visible 96 %96 %Solar Transmission; ASTM E-424
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Dimensional Stability1% shrinkage.MD. 30 minutes at 150°C
 1% shrinkage.TD. 30 minutes at 150°C
Heat of Combustion5.3 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)1000ASTM B117. 5% NaCl at 35 °C (95 °F).
Tear Strength-Initial (Graves)500 gASTM D1004
Tear Strength-Propagating (Elmendorf)75 gASTM D 1922
Weather Resistance (years unaffected)10Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8846 / 268773

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.