MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Label-Lyte® 440 LL-201 Matte Finish, Clear OPP Overlaminate  (discontinued **)
Categories: Polymer; Adhesive; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Matte finish, clear, polypropylene film intended for uses as an overlaminate in pressure-sensitive labeling applications. It presents an appealing paper-like, matte appearance while providing the benefits of a typical film overlaminate, including protected print, crisp graphics and moisture resistance.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 17.8 microns0.700 mil
Coating Weight >= 15.7 g/m²>= 9.80 lb/ream520
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 200 %200 %510
Film Elongation at Break, TD 60 %60 %510
Film Tensile Strength at Break, MD 118.20 MPa17143 psi510
Film Tensile Strength at Break, TD 265.94 MPa38571 psi510
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 5.0 %
@Temperature 135 °C
5.0 %
@Temperature 275 °F
438
Shrinkage, TD 5.0 %
@Temperature 135 °C
5.0 %
@Temperature 275 °F
438
 
Optical PropertiesMetricEnglishComments
Haze 70 %70 %444
Gloss 10 %10 %442
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Descriptive Properties
Wetting Tension, receding COS theta0.88
Yield, in2/lb44000

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEXB463 / 37768

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.