Melinex® 526 is a high clarity polyester film, with a standard T-sub pretreatment on one surface that promotes adhesion to many vinyl and acrylic based inks and to most solvent coating formulations. The other surface is pretreated with an RHI antistat. This film has balanced shrinkage.Information provided by DuPont. |