MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dymax 9003v3.0 Flexible Clear Microencapsulant
Categories: Polymer; Adhesive; Thermoset

Material Notes:
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9003v3.0 Flexible Clear Microencapsulant
Glob top for photosensing devices Cure Type: UV/Visible Typical Use: Optical potting

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 45000 cP45000 cP
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0833 - 0.250 min0.00139 - 0.00417 hour10-20 mil thick layers cured with Dymax 5000-EC at 2 inches. Thicker layers may require more cure time.
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dymax 910 Strain Relief, Wire and Parts Tacking Adhesive
Dymax 914-A Strain Relief, Wire and Parts Tacking Adhesive
Henkel Loctite® SpeedBonder™ 325 High Temperature Acrylic Bonding Adhesive
Dymax Ultra Fast™ 3-3095 Tack Gel Adhesive
Master Bond MB297Med-1 Ethyl Cyanoacrylate

PDYYMAX56 / 35040

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.