MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Ultramid® A3Z HP UN Nylon 66, Impact Modified
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Ultramid A3Z HP UN is an unreinforced, impact modified, heat stabilized, high flow PA66 injection molding grade. Ultramid A3Z HP UN offers a unique combination of maximum toughness and impact resistance with excellent high flow processability.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 MPa7250 psiDry; ISO 527
Elongation at Break 45 %45 %Dry, Nominal; ISO 527
 >= 50 %>= 50 %Conditioned, Nominal; ISO 527
Elongation at Yield 5.0 %5.0 %Dry; ISO 527
Tensile Modulus 1.06 GPa154 ksiConditioned; ISO 527
 1.90 GPa276 ksiDry; ISO 527
Flexural Modulus 0.880 GPa128 ksiConditioned; ISO 178
 1.80 GPa261 ksiDry; ISO 178
Izod Impact, Notched (ISO)  18.0 kJ/m²
@Temperature -40.0 °C
8.57 ft-lb/in²
@Temperature -40.0 °F
Dry; ISO 180
 23.0 kJ/m²
@Temperature -40.0 °C
10.9 ft-lb/in²
@Temperature -40.0 °F
Dry; ISO 180
 80.0 kJ/m²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 180
 99.0 kJ/m²
@Temperature 23.0 °C
47.1 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 180
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179
Charpy Impact, Notched  1.90 J/cm²
@Temperature -30.0 °C
9.04 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179
 2.80 J/cm²
@Temperature -30.0 °C
13.3 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179
 11.3 J/cm²
@Temperature 23.0 °C
53.8 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDry; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 170 °C338 °FDry; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C147 °FDry; ISO 75
UL RTI, Electrical  140 °C
@Thickness 0.750 mm
284 °F
@Thickness 0.0295 in
UL746B
 140 °C
@Thickness 3.00 mm
284 °F
@Thickness 0.118 in
UL746B
UL RTI, Mechanical with Impact  105 °C
@Thickness 0.750 mm
221 °F
@Thickness 0.0295 in
UL746B
 105 °C
@Thickness 3.00 mm
221 °F
@Thickness 0.118 in
UL746B
UL RTI, Mechanical without Impact  110 °C
@Thickness 0.750 mm
230 °F
@Thickness 0.0295 in
UL746B
 110 °C
@Thickness 3.00 mm
230 °F
@Thickness 0.118 in
UL746B
Flammability, UL94 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 288 - 305 °C550 - 581 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature 60.0 °C
@Time 3600 - 7200 sec
140 °F
@Time 1.00 - 2.00 hour
Moisture Content 0.040 - 0.20 %0.040 - 0.20 %
Injection Pressure 34.5 - 124 MPa5000 - 18000 psi
Back Pressure 0.000 - 50.0 MPa0.000 - 7250 psi
Screw Speed 40 - 80 rpm40 - 80 rpm
 
Descriptive Properties
Compression Ratio3:1-4:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8954 / 254912

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.