MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zinc Tin Arsenide, ZnSnAs2
Categories: Ceramic; Phosphide/Pnictide; Other Engineering Material; Semiconductor

Key Words: Pnictide; Semiconductor; Arsenic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.53 g/cc
a Lattice Constant 5.8515 Å
c Lattice Constant 11.704 Å
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 4550N/mm²
 
Electrical PropertiesOriginal ValueComments
Magnetic Susceptibility -0.0000184Atomic (cgs)
Band Gap 0.65 eV
Hole Mobility, cm²/V-s 300
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 15.0 W/m-K
Melting Point 775 °CDisorders at 637°C
Heat of Formation 252 kJ/mol
Debye Temperature -2.00 °C
 
Descriptive Properties
Crystal StructureTetragonalChalcopyrite Structure - Space Group I(-4)2d

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zinc Tin Antimonide, ZnSnSb2
Zinc Tin Arsenide, ZnSnAs2, High Temperature Form
Tin Telluride, SnTe
Zinc Tin Phosphide, ZnSnP2, Cubic
Zinc Tin Phosphide, ZnSnP2, Tetragonal

DSEN79 / 3088

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.