The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications. Key Features and Benefits: - A Proven High-Tg Substrate
- Robust Thermal Properties
- Superior electrical properties
- Enhanced Standard FR-4 processing
Applications/Qualifications: - Fine-Line Multilayers
- Backplanes
- Surface-Mount Multilayers
- BGA Multilayers
- CSP Attachment
- Automotive
- Underhood Automotive
- Wireless Communications
- Infrastructure
- Network Storage
- High-End Servers
- RoHS Compliant
- Meets IPC-4101/24 and /26 Specifications
Information provided by Park Electrochemical Corp. |