Applications: cryogenic environment applicationsterminationssever wedgesload pelletsabsorbersFeatures: dielectric loss independent from temperature. Information provided by Ceradyne Company Ceradyne was acquired by 3M in 2012. The product line has been extensively renamed and reconfigured. |