MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Momentive Performance Materials GE Sealants & Adhesives Paintable Silicone Supreme Window & Door Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: Paintable Silicone Supreme Window & Door sealant is a premium sealant with a hybrid formulation that combines the outstanding waterproof performance you would expect from a silicone sealant with the ease of use and paintable of an acrylic latex. This 100% waterproof sealant is ideal for a variety of exterior and weatherproofing projects and interior applications. It can be exposed to water or painted in as little as 30 minutes. Paintable Silicone Supreme Kitchen & Bath sealant offers 10-year mold-free product protection, has long-lasting durability, and is low odor. This sealant is permanently flexible, will not break down due to severe weather and won’t crack or crumble over time. Backed by a lifetime guarantee.

Features: Hybrid performance, waterproof and paintable, 100% waterproof, 30-minute rain-ready, 30-minute paint-ready, Resists mold with 10-year mold-free product protection • Permanent flexibility, Excellent adhesion to wet or dry surfaces, Shrink & crack-proof, Low odor, Meets ASTM C-920 Class 25 specifications, Lifetime guarantee.

Applications: Paintable Silicone Supreme Window & Door sealant is used in a wide variety of applications including windows, doors, siding, trim, decks, lattice, soffits, and vents.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccCured.
Volatile Organic Compounds (VOC) Content <= 21 g/l<= 21 g/lUncured. Excluding water & exempt compounds; WPSTM C1454
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2929ASTM D2240
Tensile Strength 0.896 MPa130 psiASTM D412
Elongation at Break 210 %210 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 65.6 °C150 °F
Minimum Service Temperature, Air -34.4 °C-30.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hour1/4" deep section
 7200 - 10100 min120 - 168 hourFull Cured. Most common bead sizes.
Tack-Free Time 30.0 min0.500 hour50% RH; ASTM C679
Working Life 20.0 min20.0 min
 
Descriptive Properties
AppearancePaste
Carb Chem Curing VOC< 3.0 wt%
ColorwhiteM90026-30
Consistency / Sag< 0.01 inchesASTM D2202
Joint Movement Capability±25%ASTM C719.
OdorLow
Rain Ready30 minutes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9944 / 265755

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.