MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® C 218L V30 PA6, 30% glass fiber, Eh 0
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL C 218 L V30 is a polyamide 6 reinforced with 30% glass fiber and UV stabilized.

Colors: it is marketed in the natural and black color.

Available in: Latin America

Main Properties: ? Excellent superficial aspect, Excellent dimensional stability, Good thermal resistance,? UV stabilization and Good impact resistance

Applications: TECHNYL C 218 L V30 was developed for applications where good balance of mechanical and thermal properties are required with good superficial aspect.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccISO 1183/A
Water Absorption 0.95 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Maximum Moisture Content <= 0.20
Linear Mold Shrinkage, Flow 0.035 cm/cm
Linear Mold Shrinkage, Transverse 0.065 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 165 MPaISO 527
Elongation at Break 3.8 %ISO 527
Tensile Modulus 9700 MPaISO 527
Flexural Strength 230 MPaASTM D790
Flexural Modulus 14300 MPaISO 178
Izod Impact, Notched 110 J/mASTM D256
Charpy Impact Unnotched 70.0 kJ/m²ISO 179
Charpy Impact, Notched 8.00 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmCEI 93
Dielectric Constant 3.8CEI 250
Dissipation Factor 0.020CEI 250
Comparative Tracking Index 550 VCEI 112
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °C
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 208 °CISO 75/Af
Flammability, UL94 HB
Oxygen Index 23 %ISO 4589
Glow Wire Test 650 °CISO 60695
 
Processing PropertiesOriginal ValueComments
Feed Temperature 230 - 235 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 80.0 °C
 
Descriptive Properties
Compression Zone230-240°C
Mixing Zone240-250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epsan Eplamid 6 GFR 30 NC HF Q1D002 Polyamide 6
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry)
Ashley Polymers Ashlene® 830LS-30G Nylon 6, 30% Glass Reinforced
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled
Envalior Akulon® K224-G6 PA6-GF30, Dry, 30% Glass Filled

PRHOD775 / 138006

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.