MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling SUSTAPEEK® M PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes:

Information provided by Röchling.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ASTM D792
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ASTM D570
Water Absorption at Saturation 0.50 %0.50 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 105105ASTM D785
Hardness, Rockwell R 126126ASTM D785
Hardness, Shore D 8585ASTM D2240
Tensile Strength, Yield 110 MPa16000 psiASTM D638
Elongation at Break 20 %20 %ASTM D638
Tensile Modulus 3.45 GPa500 ksiASTM D638
Flexural Strength 172 MPa25000 psiASTM D790
Flexural Modulus 4.14 GPa600 ksiASTM D790
Izod Impact, Notched 0.641 J/cm1.20 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.8 µm/m-°C26.0 µin/in-°FASTM D696
Thermal Conductivity 0.249 W/m-K1.73 BTU-in/hr-ft²-°F
Melting Point 332 °C630 °FASTM D789
Maximum Service Temperature, Air 249 °C480 °F
Deflection Temperature at 0.46 MPa (66 psi) 182 °C360 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
NSF NoNo
USDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450G™ General Purpose
VICTREX™ PEEK 450G903 Black Polyetheretherketone, Unreinforced
VICTREX™ PEEK 450CA30 30% Carbon Fiber Reinforced
VICTREX™ PEEK 380P Polyetheretherketone, Unreinforced
VICTREX™ PEEK 150XF Polyetheretherketone, Unreinforced

PROCH9057 / 232760

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.