MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Multibase Multi-Flex® TPO D 3105
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: The following is the actual data obtained from the above sample number. This material is based on new generation TPO technology. It has been designed for use as the first shot for airbag covers.

Data provided by Multibase.

Key Words: Thermoplastic Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.904 g/ccASTM D792-91
Linear Mold Shrinkage 0.0124 cm/cmASTM D955-95
Melt Flow 2.7 g/10 min(Condition L) ASTM D-1238-94a
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 3910 sec; ASTM D-2240-95
Tensile Strength, Ultimate 15.8 MPaASTM D638-95
Elongation at Break 540 %ASTM D638-95
Flexural Modulus 0.177 GPaMethod 1, Proc. B; ASTM D-790-95
Izod Impact, Notched NBASTM D-256-93a
Tear Strength 84.0 kN/mASTM D624-95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Multibase Multi-Flex® TPO D-5016
LyondellBasell Plexar PX2600 Polyolefin
LyondellBasell Microthene MN72700 Polyolefin
LyondellBasell Hifax™ CB259 Thermoplastic Polyolefin Elastomer
LyondellBasell Hifax™ CA260GC Thermoplastic Polyolefin Elastomer

PLA210 / 49607

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.