MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zircar Refractory Composites ASPA-880 Alumina-Silica Fiber Paper
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: ASPA-880 is a high temperature, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. It is made from shorter and smaller diameter fibers with a higher alumina content and are laid up at significantly higher density. These factors lead to high temperature, slow shrinkage, higher strength, and better chemical resistivity. This alumina-silica fiber paper exhibit very low thermal conductivity and is designed for use in applications where flexibility, high strength and resistance to heat are paramount. Type ASPA-880 exhibits low thermal conductivity and is ideal for applications up to 1450°C (2642°F). It is used in environments where standard ceramic fiber papers will not survive.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.280 g/cc0.0101 lb/in³
Loss On Ignition 8.0 %8.0 %
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0800 W/m-K
@Temperature 500 °C
0.555 BTU-in/hr-ft²-°F
@Temperature 932 °F
 0.120 W/m-K
@Temperature 800 °C
0.833 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 0.140 W/m-K
@Temperature 871 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 1600 °F
 0.160 W/m-K
@Temperature 1100 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 2010 °F
Melting Point 1930 °C3510 °F
Maximum Service Temperature, Air 1450 °C2640 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 55 %55 %
Other 1.0 %1.0 %
SiO2 44 %44 %
 
Descriptive Properties
ColorWhite
Fiber Index, %45
Mullen Burst, psi37
Tensile Strength, g/in6500
Type of BinderOrganic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-201 Refractory Sheet
Zircar Refractory Composites RSLE-57 Refractory Sheet
Zircar Refractory Composites RS-200 Refractory Sheet
Crystex Composites Mykroy/Mycalex MM 1301 Molding Grade Glass-bonded Mica Composite
Thermal Transfer Composites PRIMEX Cast™ MCX-1405™ Aluminum Silicon Carbide Composite, Reinforced

CZRCI05 / 2868

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.