MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parabeam Industrie ParaTank 6 3D Glass Fabric
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Core Material; Composite Fibers

Material Notes: Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the decklayers thus forming an integral sandwich structure.
When the Parabeam® is impregnated with a thermoset resin, the fabric absorbs the resin and due to the capillary forces of the piles, the fabric rises to the preset height.
In this one-step process a lightweight and strong sandwich laminate is formed that offers excellent mechanical properties. Parabeam® can be used for many applications in the composite industry while offering multiple advantages against traditional sandwiches and solid laminates such as woods, foams, balsa, honeycombs and more.

Information provided by the manufacturer, Parabeam Industrie, The Netherlands.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength >= 4.00 MPa>= 580 psiASTM C365
 4.00 MPa580 psiTypical; ASTM C365
Shear Modulus >= 0.0200 GPa>= 2.90 ksiASTM C273
 0.0600 GPa8.70 ksiTypical; ASTM C273
Shear Strength >= 1.00 MPa>= 145 psiASTM C273
 2.30 MPa334 psiTypical; ASTM C273
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0600 W/m-K0.416 BTU-in/hr-ft²-°FDIN 52616

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cymat A35620SC 040SS Stabilized Aluminum Foam
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System
Overview of materials for 5000 Series Aluminum Alloy
Overview of materials for 3000 Series Aluminum Alloy
Milliken® VelaCarb 335 Carbon Fiber Fabric

CPB3D110 / 1704

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.