MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay Amyl Acid Phosphate
Categories: Fluid

Material Notes: Identification: AMYL ACID PHOSPHATE - Phosphoric acid, mono – and bis –(branched and linear pentyl esters)

CAS: 84418 – 71 – 3

Available in: Asia Pacific, Europe, Latin America and North America

Solubility: Soluble in common organic solvents and slightly soluble in water

Applications: Amyl Acid Phosphate can be employed in many applications such as acid catalysts in coatings, dispersants, lubricants and antistatic agent in textile manufacture.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 - 1.10 g/cc0.0383 - 0.0397 lb/in³AV15
pH <= 2.0<= 2.0saturated aqueous solution
Viscosity 200 cP200 cP
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 410 - 490410 - 490[mg KOH/g], Direct; AV161
 
Thermal PropertiesMetricEnglishComments
Melting Point <= -15.0 °C<= 5.00 °FFreezing Point
Flash Point >= 92.0 °C>= 198 °FClosed cup; AM6511
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceColorless to pale yellow liquid
CompositionPhosphorus content14-16%, AV162
 Pyrophosphate<2.0%, AM6520

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WRHOD294 / 137525

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.