MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Palm Labs Adhesives TURBO-LOCK SERIES 17-HT Anaerobic Thread Locking Compound
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: BEARING AND SHAFT - SERIES 17-HT is a fast curing, GREEN, high temperature, high strength, high viscosity, press fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly resistance to high heat, vibrations, water, gases, oils, hydrocarbons and many chemicals.

Applications:

  • Ideal to fill gaps up to 0.015”
  • Excellent for slip fitting parts.
  • Withstands working temperatures up to 450ºF
  • Retaining sleeves, pulleys, gears, rotors and fans on shafts.
  • Mounting sleeves, securing bushings, bearings and plugs in housing.
  • Excellent retaining and sealing compound

Part Numbers for this data: 17-001-HT, 17-010-HT, 17-050-HT, 17-250-HT, 17-1000-HT

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 923-26-2, 15625-89-5, 79-10-7, 80-15-9 and 114-83-0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/cc
Brookfield Viscosity 8400 cP8400 cPRVT Spindle 3 @ 20 rpm
 
Mechanical PropertiesMetricEnglishComments
Shear Strength  13.0 - 15.0 MPa
@Temperature 22.0 °C,
Time 108000 sec
1890 - 2180 psi
@Temperature 71.6 °F,
Time 30.0 hour
ISO 10123; Compressive, Steel pins and collars
 17.0 - 19.0 MPa
@Temperature 22.0 °C,
Time 86400 sec
2470 - 2760 psi
@Temperature 71.6 °F,
Time 24.0 hour
ISO 10123; Compressive, Steel pins and collars
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FASTM D696
Specific Heat Capacity 0.300 J/g-°C0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 450 °C842 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
Flash Point 33.9 °C93.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min0.500 hourHandling
 120 - 240 min2.00 - 4.00 hourFunctional
 1440 min24.0 hourFull
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceGreen
Chemical Resistance100% Initial Strength RetainedEthanol at 22°C, at 500hrs
 100% Initial Strength RetainedMotor Oil at 125°C, at 500hrs
 100% Initial Strength RetainedGasoline at 22°C, at 500hrs
 100% Initial Strength RetainedBrake Fluid at 22°C, at 500hrs
 100% Initial Strength RetainedEthanol at 22°C, at 1000hrs
 100% Initial Strength RetainedMotor Oil at 125°C, at 1000hrs
 100% Initial Strength RetainedGasoline at 22°C, at 1000hrs
 100% Initial Strength RetainedBrake Fluid at 22°C, at 1000hrs
 80% Initial Strength RetainedWater/Glycol at 87°C, at 1000hrs
 85% Initial Strength RetainedWater/Glycol at 87°C, at 500hrs
 90% Initial Strength RetainedAcetone at 22°C, at 1000hrs
 95% Initial Strength RetainedAcetone at 22°C, at 500hrs
CompositionUrethane Methacrylate
Gap Fill0.015"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPALML052 / 135206

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.