MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ASTM A148 Grade 105-85 Cast Steel
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: High Strength Castings for Structural Purposes

Key Words: 725-585, D50850, SAE 8625
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 250
Tensile Strength, Ultimate 830 MPa
Tensile Strength, Yield 660 MPa
Elongation at Break 19 %
Reduction of Area 39 %
Modulus of Elasticity 190 GPa
Poissons Ratio 0.29
Fatigue Strength 450 MPa
Shear Modulus 73.0 GPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.0000203 ohm-cmequal weight 8.5 % IACS
 0.0000233 ohm-cmequal volume 7.4 % IACS
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 250 J/g
CTE, linear 13.0 µm/m-°C
Specific Heat Capacity 0.470 J/g-°C
Thermal Conductivity 39.0 W/m-K
Melting Point 1420 °Csolidus
 1460 °Cliquidus
Maximum Service Temperature, Air 420 °Cmax mechanical
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.20 - 0.30 %
Chromium, Cr 0.40 - 0.80 %
Iron, Fe 96.2 - 98.3 %
Manganese, Mn 0.60 - 0.90 %
Molybdenum, Mo 0.15 - 0.30 %
Nickel, Ni 0.40 - 0.80 %
Phosphorus, P <= 0.050 %
Silicon, Si <= 0.60 %
Sulfur, S <= 0.060 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MASTMA148a / 313985

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.