MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Colmant Coated Fabrics SBR Coated Aramid Fabric
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: The aramid fabric coated with SBR combines the following characteristics: Styrene Butadiene Rubber, mostly known as SBR, is one of the best options when applied to general purposes. Compared to natural rubber, SBR shows better abrasion resistance and heat-aging properties. Though, the resilience and the physical properties tend to be lower than those of Natural Rubber. Fiber consisting of a long chain polymer containing amines and aromatic components. Infusible, does not melt, does not burn, does not soften. Besides it shows low emission of toxic gases while combustion. Certain aramid can decompose at 500° C, It is thermostable up to 250° C.

Applications:

  • High temperature filtration
  • Clothing fire protection
  • Bullet proof vest
  • Thermo industry, electric and electronic
  • Aerospace industry, Shoe soles, tires
Properties:
  • Fireproofed
  • Abrasion resistance
  • Non-skid

Information provided by COLMANT COATED FABRICS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30 - 9030 - 90
Tensile Strength at Break 8.00 - 20.0 MPa1160 - 2900 psi
Elongation at Break 100 - 900 %100 - 900 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Descriptive Properties
IRHD Hardness30-90
Point Temperature-50 C° - 90°C
Warp breaking strength350 - 5000 daN/5cm
Warp elongation at break2% - 5%
Weft breaking strength350 - 2000 daN/5cm
Weft elongation at break2% - 5%
Weight per sqm100 - 650

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOLMANT060 / 316110

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.