Formolene® 5147L is a highly isotactic, nucleated polypropylene homopolymer designed for applications requiring very high stiffness. Applications have included thermoforming of containers requiring high top loading strength. Material has also found good usage in compounding applications. Formolene® 5147L meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact.Information provided by Formosa Plastics Corporation, U.S.A. |