MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Lotte Advanced Materials Infino® NH-1017 PC/ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes:

Information provided by Lotte Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccNatural or representative color; ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0030 in/in
@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 55 g/10 min
@Load 10.0 kg,
Temperature 220 °C
55 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 113113ASTM D785
Tensile Strength at Break 43.1 MPa6250 psi50 mm/min; ASTM D638
Tensile Strength, Yield 53.0 MPa7680 psi50 mm/min; ASTM D638
Elongation at Break 8.8 %8.8 %50 mm/min; ASTM D638
Tensile Modulus 2.35 GPa341 ksi50 mm/min; ASTM D638
Flexural Strength 73.5 MPa10700 psi2.8 mm/min; ASTM D790
Flexural Modulus 2.06 GPa299 ksi2.8 mm/min; ASTM D790
Izod Impact, Notched 4.41 J/cm
@Thickness 3.17 mm
8.27 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
@Thickness 6.40 mm
189 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
@Thickness 6.40 mm
176 °F
@Thickness 0.252 in
ASTM D648
Vicat Softening Point 91.0 °C196 °FB/50; ISO R 306
UL RTI, Electrical 85.0 °C
@Thickness 2.00 mm
185 °F
@Thickness 0.0787 in
UL 746B
UL RTI, Mechanical with Impact 85.0 °C
@Thickness 2.00 mm
185 °F
@Thickness 0.0787 in
UL 746B
UL RTI, Mechanical without Impact 85.0 °C
@Thickness 2.00 mm
185 °F
@Thickness 0.0787 in
UL 746B
Flammability, UL94  V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 5VB
@Thickness 2.00 mm
5VB
@Thickness 0.0787 in
 5VB
@Thickness 3.00 mm
5VB
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® NH-1021U PC/ABS
Lotte Advanced Materials Infino® NE-1030TV PC/ABS
Lotte Advanced Materials Infino® NE-1030 PC/ABS, Unreinforced FR
Lotte Advanced Materials Infino® NH-1001T PC/ABS, Unreinforced FR
Lotte Advanced Materials Infino® NH-1021 PC/ABS, Unreinforced FR

PLOTT9853 / 205715

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.