MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Gneiss
Categories: Ceramic

Material Notes: Metamorphic rock, resembling granite in appearance. The grains in gneiss have grown into a parallel structure; its compressive strength is higher perpendicular to the grain axes than parallel to this axis.

Property values are typical of Gneiss used in construction. Actual property values will vary from sample to sample.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.24 - 3.36 g/cc
Porosity 0.50 - 1.5 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore H 74 - 97
Hardness, Mohs 5.26 - 6.47
Tensile Strength, Ultimate 5.00 - 20.0 MPa
Modulus of Elasticity 13.0 - 35.0 GPa
Modulus of Rupture 0.00830 - 0.0214 GPa
Flexural Strength 10.0 - 20.0 MPa
Transverse Strength 8.00 - 21.0 MPa
Compressive Strength 22000 - 36000 psi
Impact Toughness 3.70 - 8.40 in/in²
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 10000 - 1.00e+10 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.30 - 4.40 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.736 - 0.816 J/g-°C
Thermal Conductivity 2.10 - 3.40 W/m-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandstone, Medium
Granite
Gabbro
Marble
Basalt

BMIN046 / 195

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.