MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Westlake EC 480 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Applications
  • Milk Cartons
  • Liquid Containers
  • Multiwall Bag Stock
  • Frozen Food Containers
Properties
  • Good Drawdown
  • Excellent Adhesion to Substrates
  • Very Good Heat Sealability
  • Very Good Moisture Barrier

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520, paragraph C, section 2.1, for use in articles that contact food. Kosher approved

Processing: The very good flow properties of Westlake Polymers EC 480 permit high-speed coatings at weights from 4 lbs. / 3,000 sq. ft. and up. Suggested melt temperatures range for extrusion coating EC 480 is 575° to 625°F.

Information provided by Westlake Chemical Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ASTM D1505
Water Vapor Transmission 15.5 g/m²/day
@Temperature 37.8 °C
0.998 g/100 in²/day
@Temperature 100 °F
ASTM D96(E)
Oxygen Transmission 197 cc-mm/m²-24hr-atm500 cc-mil/100 in²-24hr-atmASTM D1434
Nitrogen Transmission 78.7 cc-mm/m²-24hr-atm200 cc-mil/100 in²-24hr-atmASTM D1434
Carbon Dioxide Transmission 709 cc-mm/m²-24hr-atm1800 cc-mil/100 in²-24hr-atmASTM D1434
Melt Flow 4.5 g/10 min4.5 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 12.4 MPa1800 psiASTM D638
Elongation at Break 580 %580 %ASTM D638
Tensile Modulus 0.125 GPa18.2 ksiASTM D1709
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 100 °C212 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 302 - 329 °C575 - 625 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Riblene® MM 20 Low Density Polyethylene - Injection Molding
Carmel Olefins Ipethene® 670 Low Density Polyethylene
Carmel Olefins Ipethene® 600 Low Density Polyethylene
Braskem PB 608 LDPE Injection Molding Polyethylene
Braskem PB 208 LDPE Injection Molding Polyethylene

PWESG031 / 72677

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.