MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV 24824 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink 24824 is a very low durometer thermoplastic vulcanizate designed for industrial applications. This grade is a low hardness, low density, lubricated grade suitable for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Light Stabilized; Low Density; Low Flow; Low Hardness; Low Specific Gravity; Lubricated; Slip

Uses: Expansion Joint; Gaskets; Grommets; Plugs; Shock Absorbing Pads; Tubing; Weatherstripping

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  26
@Time 5.00 sec
26
@Time 0.00139 hour
Injection Molded; ASTM D2240
 30
@Time 1.00 sec
30
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 2.32 MPa336 psiFlow, Die C, 20 in/min; ASTM D412
 2.55 MPa370 psiAcross Flow, Die C, 20 in/min; ASTM D412
Tensile Stress at Strain  0.648 MPa
@Strain 100 %
94.0 psi
@Strain 100 %
Across Flow, Die C, 20 in/min; ASTM D412
 0.669 MPa
@Strain 100 %
97.0 psi
@Strain 100 %
Flow, Die C, 20 in/min; ASTM D412
 1.73 MPa
@Strain 300 %
251 psi
@Strain 300 %
Flow, Die C, 20 in/min; ASTM D412
 1.75 MPa
@Strain 300 %
254 psi
@Strain 300 %
Across Flow, Die C, 20 in/min; ASTM D412
Elongation at Break 390 %390 %Flow, Die C, 20 in/min; ASTM D412
 410 %410 %Across Flow, Die C, 20 in/min; ASTM D412
Tear Strength 9.29 kN/m53.0 pliAcross Flow, Die C, 20 in/min; ASTM D624
 9.47 kN/m54.0 pliFlow, Die C, 20 in/min; ASTM D624
Compression Set  10 %
@Temperature 22.8 °C,
Time 79200 sec
10 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395
 27 %
@Temperature 70.0 °C,
Time 79200 sec
27 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 50.0 °C122 °FUL 746
UL RTI, Mechanical with Impact 50.0 °C122 °FUL 746
UL RTI, Mechanical without Impact 50.0 °C122 °FUL 746
Flammability, UL94 HB
@Thickness 1.52 - 1.78 mm
HB
@Thickness 0.0600 - 0.0700 in
All Colors
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 230 °C374 - 446 °FInjection, Melt
Rear Barrel Temperature 173 - 213 °C344 - 416 °FInjection
Middle Barrel Temperature 179 - 219 °C354 - 426 °FInjection
Front Barrel Temperature 184 - 224 °C364 - 436 °FInjection
Nozzle Temperature 190 - 230 °C374 - 446 °FInjection
Zone 1 166 - 204 °C330 - 400 °FExtrusion
Zone 2 171 - 210 °C340 - 410 °FExtrusion
Zone 3 177 - 216 °C350 - 420 °FExtrusion
Zone 4 179 - 218 °C355 - 425 °FExtrusion
Zone 5 182 - 221 °C360 - 430 °FExtrusion
Die Temperature 190 - 227 °C374 - 440 °FExtrusion
Mold Temperature 35.0 - 60.0 °C95.0 - 140 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 120 rpm50 - 120 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1197 / 237688

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.