MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem AKROCHEM® C595 RESIN Resin
Categories: Polymer; Thermoplastic

Material Notes: Product Description: C595 Resin is a light colored C5 type resin which provides superior tackifying action to synthetic and natural rubber applications.

Applications: C595 Resin aids in processing elastomers and plastic products by increasing green tack, rate of incorporation of fillers and pigments, and provides wetting action for fillers. In addition, C595 Resin improves rubber to metal/fibers bonding. Common applications include hot melt adhesives, general tackifier and/or softener in NR and synthetic elastomers.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Ash <= 0.10 %
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.50[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Softening Point 90.0 - 100 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 7.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH378 / 315296

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.