MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPE RV-2670D Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink RV-2670D is a high performance thermoplastic elastomer, available in NAT and BLK, used in a variety of transportation applications. Sarlink RV-2670D is a high hardness, high density, filled grade with a 400k psi modulus that is UV stabilized and suitable for extrusion and injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Filled; Good Adhesion; Good Toughness; High Density; High Hardness; High Specific Gravity; Low Flow; Lubricated; Sunlight Resistant; Slip; UV Resistant; Weather Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Racks

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Viscosity 613 cP
@Shear Rate 206 1/s,
Temperature 200 °C
613 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  68
@Time 15.0 sec
68
@Time 0.00417 hour
Injection Molded; ISO 868
 69
@Time 5.00 sec
69
@Time 0.00139 hour
Injection Molded; ISO 868
 70
@Time 1.00 sec
70
@Time 0.000278 hour
Injection Molded; ISO 868
 69.3
@Treatment Temp. 125 °C,
Time 15.0 sec
69.3
@Treatment Temp. 257 °F,
Time 0.00417 hour
Change in Air, 168 hr; ISO 888
 69.4
@Treatment Temp. 110 °C,
Time 15.0 sec
69.4
@Treatment Temp. 230 °F,
Time 0.00417 hour
Change in Air, 1008 hr; ISO 888
 70.1
@Treatment Temp. 125 °C,
Time 1.00 sec
70.1
@Treatment Temp. 257 °F,
Time 0.000278 hour
Change in Air, 168 hr; ISO 888
 70.1
@Treatment Temp. 125 °C,
Time 5.00 sec
70.1
@Treatment Temp. 257 °F,
Time 0.00139 hour
Change in Air, 168 hr; ISO 888
 70.2
@Treatment Temp. 110 °C,
Time 5.00 sec
70.2
@Treatment Temp. 230 °F,
Time 0.00139 hour
Change in Air, 1008 hr; ISO 888
 70.6
@Treatment Temp. 110 °C,
Time 1.00 sec
70.6
@Treatment Temp. 230 °F,
Time 0.000278 hour
Change in Air, 1008 hr; ISO 888
Tensile Strength at Break 17.9 MPa2590 psiAcross Flow, Type 1, 20 in/min; ISO 37
 21.8 MPa3160 psiFlow, Type 1, 20 in/min; ISO 37
 18.6 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
2690 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Type 1, Change in Air; ISO 188
 18.9 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
2750 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Type 1, Change in Air; ISO 188
 23.5 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
3410 psi
@Treatment Temp. 257 °F,
Time 168 hour
Flow, Type 1, Change in Air; ISO 188
 24.2 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
3510 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain  12.8 MPa
@Strain 100 %
1850 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 17.2 MPa
@Strain 100 %
2500 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 14.8 MPa
@Strain 100 %,
Treatment Temp. 110 °C
2150 psi
@Strain 100 %,
Treatment Temp. 230 °F
Across Flow, Type 1, Change in Air, 1008 hr; ISO 188
 15.3 MPa
@Strain 100 %,
Treatment Temp. 125 °C
2220 psi
@Strain 100 %,
Treatment Temp. 257 °F
Across Flow, Type 1, Change in Air, 6.61 in; ISO 188
 22.2 MPa
@Strain 100 %,
Treatment Temp. 110 °C
3230 psi
@Strain 100 %,
Treatment Temp. 230 °F
Flow, Type 1, Change in Air, 1008 hr; ISO 188
 22.9 MPa
@Strain 100 %,
Treatment Temp. 125 °C
3330 psi
@Strain 100 %,
Treatment Temp. 257 °F
Flow, Type 1, Change in Air, 168 hr; ISO 188
Elongation at Break 120 %120 %Across Flow, Type 1, 20 in/min; ISO 37
 140 %140 %Flow, Type 1, 20 in/min; ISO 37
 82.8 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
82.8 %
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Type 1, Change in Air; ISO 188
 115 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
115 %
@Treatment Temp. 230 °F,
Time 1008 hour
Flow, Type 1, Change in Air; ISO 188
 139 %
@Treatment Temp. 125 °C,
Time 605000 sec
139 %
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Type 1, Change in Air; ISO 188
 153 %
@Treatment Temp. 125 °C,
Time 605000 sec
153 %
@Treatment Temp. 257 °F,
Time 168 hour
Flow, Type 1, Change in Air; ISO 188
Flexural Modulus 2.69 GPa390 ksiASTM D790
Tear Strength 124 kN/m710 pliFlow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
 175 kN/m1000 pliAcross Flow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
Compression Set  67 %
@Temperature 22.8 °C,
Time 79200 sec
67 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ISO 815
 93 %
@Temperature 90.0 °C,
Time 252000 sec
93 %
@Temperature 194 °F,
Time 70.0 hour
Type 1; ISO 815
 94 %
@Temperature 70.0 °C,
Time 79200 sec
94 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 232 °C380 - 450 °FInjection, Melt
Rear Barrel Temperature 193 - 232 °C380 - 450 °FInjection
Middle Barrel Temperature 193 - 232 °C380 - 450 °FInjection
Front Barrel Temperature 193 - 232 °C380 - 450 °FInjection
Nozzle Temperature 193 - 232 °C380 - 450 °FInjection
Zone 1 193 - 221 °C380 - 430 °FExtrusion
Zone 2 193 - 221 °C380 - 430 °FExtrusion
Zone 3 193 - 221 °C380 - 430 °FExtrusion
Zone 4 193 - 221 °C380 - 430 °FExtrusion
Zone 5 193 - 221 °C380 - 430 °FExtrusion
Die Temperature 193 - 221 °C380 - 430 °FExtrusion
Mold Temperature 15.6 - 43.3 °C60.0 - 110 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1128 / 237619

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.