MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics CIM Zirconia Technical Ceramic
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: A very high purity zirconia-based material, partially stabilized with yttria.

Applications: Components for a range of medical, analytical and industrial applications.

information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 6.00 g/cc
Porosity 0.00 %fully dense, nominal
Grain Size 0.20 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 45 N 87
Modulus of Elasticity 220 GPa
@Temperature 20.0 °C
Young's
Flexural Strength <= 800 MPa
@Temperature 20.0 °C
4-point
Fracture Toughness 10.0 MPa-m½
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.00e+10 ohm-cm
@Temperature 100 °C
Dielectric Constant 33
@Frequency 1e+10 Hz,
Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.610 J/g-°C
Thermal Conductivity 2.90 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
ZrO2+Y2O3 99.9 %includes HfO2
 
Descriptive Properties
Colorwhite
Thermal Shock Resistance (R1), delta T/C400
Thermal Shock Resistance (R2), W/m891

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade
CoorsTek DuraSense™ Ceramic Alumina Toughened Zirconia
CeramTec MZ 111 Zirconia, ZrO2-Y2O3
Morgan Advanced Ceramics Nilcra® Zirconia 3Y-TZP Grade Y-TZP
Overview of materials for Nylon 12

CMORF8042 / 203519

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.