MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zircar Ceramics SALI Alumina Insulation
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: SALI has been serving 1700°C low mass furnace users longer than any other alumina fiber board available today. SALI is a premium grade rigid fiber board with superior hot strength.

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.480 g/cc0.0173 lb/in³
Open Porosity 84 %84 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 2.07 MPa300 psiParallel to thickness
Compressive Yield Strength 1.31 MPa190 psiat 10% Compression, Parallel to thickness
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 µm/m-°C
@Temperature 20.0 - 1100 °C
4.44 µin/in-°F
@Temperature 68.0 - 2010 °F
Specific Heat Capacity 1.05 J/g-°C0.250 BTU/lb-°F
Thermal Conductivity  0.200 W/m-K
@Temperature 400 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 752 °F
Parallel to Thickness; ASTM C177-76
 0.310 W/m-K
@Temperature 800 °C
2.15 BTU-in/hr-ft²-°F
@Temperature 1470 °F
Parallel to Thickness; ASTM C177-76
 0.390 W/m-K
@Temperature 1400 °C
2.71 BTU-in/hr-ft²-°F
@Temperature 2550 °F
Parallel to Thickness; ASTM C177-76
Melting Point 1870 °C3400 °F
Maximum Service Temperature, Air 1700 °C3090 °F
Softening Point 1100 °C2010 °FTemperature sample yields under load of push rod in CTE determination
Shrinkage 2.0 %2.0 %SAG/Distortion, 6in. (152mm) x 1in. (25.4mm) x 1in. (25.4mm), 5in. (127mm) Span, % after 24 hrs. at 1650°C
 1.0 %
@Temperature 1650 °C,
Time 86400 sec
1.0 %
@Temperature 3000 °F,
Time 24.0 hour
Perpendicular to Thickness
 3.0 %
@Temperature 1700 °C,
Time 86400 sec
3.0 %
@Temperature 3090 °F,
Time 24.0 hour
Perpendicular to Thickness
 
Component Elements PropertiesMetricEnglishComments
Al2O3 80 %80 %
SiO2 20 %20 %
 
Descriptive Properties
BondSilica
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Ceramics AL-25/1700 Alumina Insulation
Zircar Ceramics AL-30 Alumina Insulation
Zircar Ceramics AL-30AA Alumina Insulation
Zircar Ceramics AL-30AAH Alumina Insulation
Zircar Ceramics ECO-20AA Alumina Insulation

CZIR043 / 2851

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.