  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam
Categories: Other Engineering Material; Composite Core Material; Polymer

Material Notes: AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible water absorption, and provides an excellent resistance to chemicals. A fine cell structure offers an excellent bonding surface. Compatible with most resins and manufacturing processes AIREX® C71 is ideally suited as a core material for a wide variety of lightweight sandwich structures subjected to both static and dynamic loads, and exposed to elevated temperatures during manufacturing.

Characteristics

  • outstanding strength and stiffness to weight ratios
  • High temperature resistance
  • Good impact strength
  • High fatigue resistance
  • Low resin absorption (fine cell structure)
  • Good fire performance (self-extinguishing)
  • Sound and thermal insulation
  • Good styrene resistance
  • Dimensionally stable and non biodegradable
Applications
  • Wind Energy: Rotor blades, nacelles, turbine generator housings
  • Road and Rail: Roof panels, interiors, floors, doors, partition walls, side skirts, front-ends
  • Marine: Hulls, decks, bulkheads, superstructures, engine hatches
  • Aircraft: Interiors, radomes, galley carts, general aviation (sport aircraft)
  • Recreation: Skis, snowboards, surfboards, wakeboards, canoes, kayaks
  • Industrial: Tooling, tanks, ductwork, containers, covers
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.0600 g/cc0.00217 lb/in³average; ISO 845
     0.0540 - 0.0690 g/cc0.00195 - 0.00249 lb/in³typical range; ISO 845
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength >= 1.00 MPa>= 145 psiin the plane; ISO 527 1-2
     1.50 MPa218 psiaverage; in the plane; ISO 527 1-2
    Elongation at Break >= 15 %>= 15 %shear; ISO 1922
     25 %25 %average; shear; ISO 1922
    Tensile Modulus >= 0.0300 GPa>= 4.35 ksiin the plane; ISO 527 1-2
     0.0420 GPa6.09 ksiaverage; in the plane; ISO 527 1-2
    Compressive Strength >= 0.850 MPa>= 123 psiperpendicular to plane; ISO 844
     0.950 MPa138 psiaverage; perpendicular to plane; ISO 844
    Compressive Modulus >= 0.0600 GPa>= 8.70 ksiperpendicular to plane; DIN 53421
     0.0700 GPa10.2 ksiaverage; perpendicular to plane; DIN 53421
    Shear Modulus >= 0.0180 GPa>= 2.61 ksiASTM C393
     0.0215 GPa3.12 ksiaverage; ASTM C393
    Shear Strength >= 0.700 MPa>= 102 psiISO 1922
     0.930 MPa135 psiaverage; ISO 1922
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity 0.0310 W/m-K0.215 BTU-in/hr-ft²-°FISO 8301
     
    Descriptive Properties
    Colorlight red

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    3A Composites Core Materials AIREX® C70.90 Universal Structural Foam
    3A Composites Core Materials AIREX® C51.60 Industrial Processing Foam
    3A Composites Core Materials BALTEK® SB.50 Structural End-Grain Balsa
    3A Composites Core Materials AIREX® C70.40 Universal Structural Foam
    3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam

    PZ3AC013 / 108502

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.