MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Johnson Matthey Alu-flo™ HT ChannelFlux™ Aluminum-Silicon Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Solder/Braze Alloy

Material Notes: Alu-flo™ HT ChannelFlux™ is an aluminum-silicon brazing filler metal incorporating a cesium-based flux into a central channel running through the product. This unique product is designed to help companies fabricating aluminum components and looking for a cost competitive option to flux cored aluminum-silicon brazing filler metals.

Benefits of Alu-flo™ HT ChannelFlux™:

  • Improved Flow
  • Improved Bonding
  • Ductile and Durable
  • Clearly Visible Flux
  • Non-corrosive Flux Residues

Alu-flo™ HT ChannelFlux™ may be used for manufacturing heating, refrigeration and air-conditioning components from aluminum alloys. It is particularly well suited for manufacturing mobile / automotive air-conditioning components. Aluminum alloys from the 3000 and 6000 ranges may be joined successfully with this product.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 575 - 585 °C
Solidus 575 °C
Liquidus 585 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 88 %
Silicon, Si 12 %
 
Descriptive Properties
FluxCesium-based polymer system containing Nocolok® Cs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AMG Aluminum Ticar® 3% Ti - 0.15% C Titanium Carbon Aluminum Rod
Aluminum 7075-T73; 7075-T735x
Aluminum 7005-W
Aluminum 7005-T6, 7005-T63, and 7005-T6351
Aleris Weldural Aluminum Alloy, 300 mm Thickness

NJMMJ9703 / 186104

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.