MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo Technyl® A238 Unfilled, Heat Stabilized, Impact Modified Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: Information provided by Rhodia; Rhodia has been acquired by Solvay.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Key Words: Polyamide 66; PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccISO 1183-A
Water Absorption 1.1 %24 Hr.; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 30 %ISO 527
Elongation at Yield 5.0 %ISO 527
Tensile Modulus 370000 psiISO 527
Flexural Strength 13800 psiISO 178
Flexural Modulus 326000 psiISO 178
Izod Impact, Notched (ISO) 3.81 ft-lb/in²ISO 180
 
Thermal PropertiesOriginal ValueComments
Melting Point 505.4 °FISO 3146-C
Deflection Temperature at 1.8 MPa (264 psi) 158 °FISO 75-2
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Feed Temperature 482 - 518 °F
Middle Barrel Temperature 500 - 536 °FCompression Zone
Front Barrel Temperature 518 - 554 °F
Melt Temperature 518 - 554 °F
Mold Temperature 140 - 194 °FSurface
Drying Temperature 176 °FDehumidifying Dryer
Dry Time 3 - 4 hour
Moisture Content <= 0.20 %
Back Pressure 50.0 - 100 psi
Fill Speed 300 - 600 mm/secPeripheral Screw Speed
 
Descriptive Properties
Injection Speed (cm3/sec)80 - 150 cm3/sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo Technyl® A218 Heat Stabilized Nylon 66
Domo TECHNYL® A 238 Black 21 N PA66, DRY
Domo Technyl® A 246M Nylon 66, Impact Grade, EH0
Domo Technyl® A 402 H1 Nylon 66
Domo Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH0

PRHO07h / 65940

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.