MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Koattro PB M 1200M Plastomer
Categories: Polymer; Thermoplastic; Polybutene

Material Notes: Koattro is a novel family of high-molecular-weight plastomers. Polybutene-1 grade Koattro PB M 1200M is a random copolymer of butene-1 with low ethylene content. Koattro PB M 1200M is primarily used as a blend component in hot melt adhesive (HMA) formulations and sealant compounds. In order to maintain mechanical integrity at higher temperatures (higher shear adhesion failure temperature or SAFT) of an HMA, it can be used in combination with a wide variety of non-polar resins and waxes. Koattro PB M 1200M helps to reduce the amount of resin needed in a HMA formulation. Applications: Hot Melt Adhesives, Polymer Modifier, Products for Use in Property Modification, Sealants.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.908 g/ccISO 1183-1
Melt Flow 1200 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 340 MPaISO 178
 
Descriptive Properties
Processing MethodInjection Molding, Melt Blown, Spunbond

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Koattro PB 0800M Polymer
Geon® Performance Solutions M1200 Molding PVC; Opaque Grade

PEQT7593 / 219230

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.