Alloy 502 is a 5% chromium, 0.5% molybdenum alloy for use as filler metal for welding low-alloy steels where response to heat treatment is required in weld. Used extensively with the gas metal arc, gas tungsten arc and submerged arc welding processes. Information provided by Universal Wire Works for their line of welding wire and filler metal. |