MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Wacker® JSD 50E Silicone Emulsion
Categories: Fluid; Polymer

Material Notes: Product description: WACKER® JSD 50E is a 50% solids silicone defoamer emulsion concentrate formulated to permit the user flexibility and economics in use that is effective in a wide range of industrial applications. WACKER® JSD 50E is based on a high molecular weight polysiloxane and silia technology. It is safe to use in high alkaline and high temperature textile applications. WACKER® JSD 50E has excellent foam knockdown.

Application: WACKER® JSD 50E has proved ideal for tackling foam in many industrial applications including its versatility as a processing auxiliary that is valued throughout the chemical industry. WACKER® JSD 50E is recommended for many industrial applications including, foam control in bleach and scour baths, in beck, jet or package dyeing, and in finish formulations.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 50 %
pH 7.0 - 10
Viscosity 800 - 2500 cP
 
Descriptive Properties
Appearancemilky-white liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9785 / 205314

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.