MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QM 270 QSI Quantum Silicones 70 Durometer Addition Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: QM 270 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin resistance. This material is a good choice for the molding of furniture, picture frames and architectural materials. QM 270 is exceptionally good where high durometer and dimensional stability are required.

Key Features:

  • High Durometer
  • Casting resin resistance
  • Fast demold time
  • Excellent dimensional stability
Main Applications:
  • Molds for architectural replication
  • Molds for polyester, epoxy resin casting, and rigid or foam polyurethane
  • Molds for technical articles and prototype
  • Molds for furniture and picture frame replication

      Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccUncatalyzed, QM 270B
 1.33 g/ccBase
Viscosity 500 cPUncatalyzed, QM 270B
 50000 cPcatalyzed with QM 270B
 75000 cPBase
Linear Mold Shrinkage <= 0.0010 cm/cmcured 72 hrs @ RT
Storage Temperature <= 38.0 °C12 months
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75cured 72 hrs @ RT
Tensile Strength 6.90 MPacured 72 hrs @ RT
Elongation at Break 110 %cured 72 hrs @ RT
Tear Strength 100 plicured 72 hrs @ RT
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 8 - 12 hourDemold time, catalyzed with QM 270B
Pot Life 70.0 minUncatalyzed, QM 270B
 
Descriptive Properties
ColorBeigeBase
 Beige catalyzed with QM 270B
 ClearUncatalyzed, QM 270B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials Silopren™ LSR 4040 Liquid Silicone Rubber - Healthcare
RTP Company PermaStat® 1500-70D  Polyester Thermoplastic Elastomer (TPE) Anti-Static - 70 Shore D
AISI 12L14 Steel, hot rolled, 19-38 mm round
Aluminum A380.0-F Die Casting Alloy
CHT Group QM 264 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material

PACC071 / 22198

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.